Skip to main content

Table 4 Compressive, tensile, and flexure strength of concrete specimens

From: Utilization of carbon nanotubes and steel fibers to improve the mechanical properties of concrete pavement

Concrete type

Compressive strength (MPa)

Tensile strength (MPa)

Flexure strength (MPa)

Control

25.06

2.32

9.18

0.025% CNTs

26.74

2.651

10.94

0.050% CNTs

29.54

2.794

11.77

0.075% CNTs

29.47

2.807

11.32